Objectives. The paradoxical migration of the femoral neck element (FNE) superomedially against gravity, with respect to the intramedullary component of the cephalomedullary device, is a poorly understood phenomenon increasingly seen in the management of pertrochanteric hip fractures with the intramedullary nail. The aim of this study was to investigate the role of bidirectional loading on the medial migration phenomenon, based on unique wear patterns seen on scanning electron microscopy of retrieved implants suggestive of FNE toggling. Methods. A total of 18 synthetic femurs (Sawbones, Vashon Island, Washington) with comminuted pertrochanteric fractures were divided into three groups (n = 6 per group). Fracture fixation was performed using the Proximal Femoral Nail Antirotation (PFNA) implant (Synthes, Oberdorf, Switzerland; n = 6). Group 1 was subjected to unidirectional compression loading (600 N), with an elastomer (70A durometer) replacing loose fracture fragments to simulate surrounding soft-tissue tensioning. Group 2 was subjected to bidirectional loading (600 N compression loading, 120 N tensile loading), also with the elastomer replacing loose fracture fragments. Group 3 was subjected to bidirectional loading (600 N compression loading, 120 N tensile loading) without the elastomer. All constructs were tested at 2 Hz for 5000 cycles or until cut-out occurred. The medial migration distance (MMD) was recorded at the end of the testing cycles. Results. The MMDs for Groups 1, 2, and 3 were 1.02 mm, 6.27 mm, and 5.44 mm respectively, with reliable reproduction of medial migration seen in all groups. Bidirectional loading groups showed significantly higher MMDs compared with the unidirectional loading group (p < 0.01). Conclusion. Our results demonstrate significant contributions of bidirectional cyclic loading to the medial migration phenomenon in
Aims. There are concerns regarding nail/medullary canal mismatch and initial stability after
Objectives. Intramedullary fixation is considered the most stable treatment for pertrochanteric fractures of the proximal femur and cut-out is one of the most frequent mechanical complications. In order to determine the role of clinical variables and radiological parameters in predicting the risk of this complication, we analysed the data pertaining to a group of patients recruited over the course of six years. Methods. A total of 571 patients were included in this study, which analysed the incidence of cut-out in relation to several clinical variables: age; gender; the AO Foundation and Orthopaedic Trauma Association classification system (AO/OTA); type of nail; cervical-diaphyseal angle; surgical wait times; anti-osteoporotic medication; complete post-operative weight bearing; and radiological parameters (namely the lag-screw position with respect to the femoral head, the Cleveland system, the tip-apex distance (TAD), and the calcar-referenced tip-apex distance (CalTAD)). Results. The incidence of cut-out across the sample was 5.6%, with a higher incidence in female patients. A significantly higher risk of this complication was correlated with lag-screw tip positioning in the upper part of the femoral head in the anteroposterior radiological view, posterior in the latero-lateral radiological view, and in the Cleveland peripheral zones. The tip-apex distance and the calcar-referenced tip-apex distance were found to be highly significant predictors of the risk of cut-out at cut-offs of 30.7 mm and 37.3 mm, respectively, but the former appeared more reliable than the latter in predicting the occurrence of this complication. Conclusion. The tip-apex distance remains the most accurate predictor of cut-out, which is significantly greater above a cut-off of 30.7 mm. Cite this article: G. Caruso, M. Bonomo, G. Valpiani, G. Salvatori, A. Gildone, V. Lorusso, L. Massari. A six-year retrospective analysis of cut-out risk predictors in
Aims. Restoration of proximal medial femoral support is the keystone in the treatment of intertrochanteric fractures. None of the available implants are effective in constructing the medial femoral support. Medial sustainable nail (MSN-II) is a novel
Fractures of the proximal femur are one of the
greatest challenges facing the medical community, constituting a
heavy socioeconomic burden worldwide. Controversy exists regarding
the optimal treatment for patients with unstable trochanteric proximal
femoral fractures. The recognised treatment alternatives are extramedullary
fixation usually with a sliding hip screw and intramedullary fixation
with a
Fractures of the proximal femur are a common clinical problem, and a number of orthopaedic devices are available for the treatment of such fractures. The objective of this study was to assess the rotational stability, a common failure predictor, of three different rotational control design philosophies: a screw, a helical blade and a deployable crucifix. Devices were compared in terms of the mechanical work (W) required to rotate the implant by 6° in a bone substitute material. The substitute material used was Sawbones polyurethane foam of three different densities (0.08 g/cm3, 0.16 g/cm3 and 0.24 g/cm3). Each torsion test comprised a steady ramp of 1°/minute up to an angular displacement of 10°.Objectives
Methods
The use of two implants to manage concomitant ipsilateral femoral
shaft and proximal femoral fractures has been indicated, but no
studies address the relationship of dynamic hip screw (DHS) side
plate screws and the intramedullary nail where failure might occur
after union. This study compares different implant configurations
in order to investigate bridging the gap between the distal DHS
and tip of the intramedullary nail. A total of 29 left synthetic femora were tested in three groups:
1) gapped short nail (GSN); 2) unicortical short nail (USN), differing
from GSN by the use of two unicortical bridging screws; and 3) bicortical
long nail (BLN), with two angled bicortical and one unicortical bridging
screws. With these findings, five matched-pairs of cadaveric femora
were tested in two groups: 1) unicortical long nail (ULN), with
a longer nail than USN and three bridging unicortical screws; and
2) BLN. Specimens were axially loaded to 22.7 kg (50 lb), and internally
rotated 90°/sec until failure.Objectives