We performed 83 consecutive cemented revision total hip arthroplasties in 77 patients between 1977 and 1983 using improved cementing techniques. One patient (two hips) was lost to follow-up. The remaining 76 patients (81 hips) had an average age at revision of 63.7 years (23 to 89). At the final follow-up 18 hips (22%) had had a reoperation, two (2.5%) for sepsis, three (4%) for dislocation and 13 (16%) for aseptic loosening. The incidence of rerevision for aseptic femoral loosening was 5.4% and for aseptic acetabular loosening 16%. These results confirm that cemented femoral revision is a durable option in revision hip surgery when improved cementing techniques are used, but that cemented acetabular revision is unsatisfactory.
The
It has been suggested that the endurance of cemented femoral reconstructions in total hip arthroplasty is affected by the creep of acrylic cement, but it is not known to what extent cement creeps under loading conditions in vivo, or how this affects load transfer. We have simulated the
We have previously shown that joint distraction and movement with a hinged external fixation device for 12 weeks was useful for repairing a large articular cartilage defect in a rabbit model. We have now investigated the results after six months and one year. The device was applied to 16 rabbits who underwent resection of the articular cartilage and subchondral bone from the entire tibial plateau. In group A (nine rabbits) the device was applied for six months. In group B (seven rabbits) it was in place for six months, after which it was removed and the animals were allowed to move freely for an additional six months. The cartilage remained sound in all rabbits. The areas of type II collagen-positive staining and repaired soft tissue were larger in group B than in group A. These findings provide evidence of
We investigated the effect of pre-heating a femoral component on the porosity and strength of bone cement, with or without vacuum mixing used for total hip replacement. Cement mantles were moulded in a manner simulating clinical practice for cemented hip replacement. During polymerisation, the temperature was monitored. Specimens of cement extracted from the mantles underwent bending or fatigue tests, and were examined for porosity. Pre-heating the stem alone significantly increased the mean temperature values measured within the mantle (+14.2°C) (p <
0.001) and reduced the mean curing time (−1.5 min) (p <
0.001). The addition of vacuum mixing modulated the mean rise in the temperature of polymerisation to 11°C and reduced the mean duration of the process by one minute and 50 seconds (p = 0.01 and p <
0.001, respectively). In all cases, the maximum temperature values measured in the mould simulating the femur were <
50°C. The mixing technique and pre-heating the stem slightly increased the static mechanical strength of bone cement. However, the fatigue life of the cement was improved by both vacuum mixing and pre-heating the stem, but was most marked (+ 280°C) when these methods were combined. Pre-heating the stem appears to be an effective way of improving the quality of the cement mantle, which might enhance the
Despite worldwide clinical use of bio-absorbable devices for internal fixation in orthopaedic surgery, the degradation behaviour and tissue replacement of these implants are not fully understood. In a
The success of
Studies on the migration of an implant may be the only way of monitoring the early performance of metal-on-metal prostheses. The Ein Bild Roentgen Analyse - femoral component analysis (EBRA-FCA) method was adapted to measure migration of the femoral component in a metal-on-metal surface arthroplasty of the hip using standard antero-posterior radiographs. In order to determine the accuracy and precision of this method a prosthesis was implanted into cadaver bones. Eleven series of radiographs were used to perform a zero-migration study. After adjustment of the femoral component to simulate migration of 3 mm the radiographs were repeated. All were measured independently by three different observers. The accuracy of the method was found to be ± 1.6 mm for the x-direction and ± 2 mm for the y-direction (95% percentile). The method was validated using 28 hips with a minimum follow-up of 3.5 years after arthroplasty. Seventeen were sound, but 11 had failed because of loosening of the femoral component. The normal (control) group had a different pattern of migration compared with that of the loose group. At 29.2 months, the control group showed a mean migration of 1.62 mm and 1.05 mm compared with 4.39 mm and 4.05 mm in the failed group, for the centre of the head and the tip of the stem, respectively (p = 0.001). In the failed group, the mean time to migration greater than 2 mm was earlier than the onset of clinical symptoms or radiological evidence of failure, 19.1 versus 32.2 months (p = 0.001) and 24.8 months (p = 0.012), respectively. EBRA-FCA is a reliable and valid tool for measuring migration of the femoral component after surface arthroplasty and can be used to predict early failure of the implant. It may be of value in determining the
Ultra-high-molecular-weight polyethylene (UHMWPE) components for total joint replacement generate wear particles which cause adverse biological tissue reactions leading to osteolysis and loosening. Sterilisation of UHMWPE components by gamma irradiation in air causes chain scissions which initiate a
Inadequate bone stock is often found in revision surgery of femoral components of total knee replacements. Our aim was to test the hypothesis that these remodelling patterns can be explained by stress shielding, and that prosthetic bonding characteristics affect maintenance of bone mass. We made a three-dimensional finite-element model of an average male femur with a cemented femoral knee component. This model was integrated with iterative remodelling procedures. Two extreme prosthetic bonding conditions were analysed and gradual changes in bone density were calculated. The
Ten acetabular cups coated with hydroxyapatite (HA) had originally been inserted in five primary and five revision total hip replacements. The thickness of the HA was 155 ± 35 μm. The cups, which were well-fixed, were retrieved, with their adherent tissue, at reoperation after 0.3 to 5.8 years because of infection (five hips), wear of polyethylene (three hips), and instability (two hips). Undecalcified sections showed a direct contact between bone and osteoid-like tissue which had formed directly onto the HA coating. The area within the threads and their mirror images, as well as the implant-tissue interfaces consisted of similar amounts of bone and soft tissue. Degradation of HA was seen in all hips. The mean thickness of the remaining HA coating was 97 μm (95% CI 94 to 101). The metal interface comprised 66% HA. The HA-tissue interface contained more bone than soft tissue (p = 0.001), whereas the metal-tissue interface included more soft tissue than bone (p = 0.019). Soft tissue at the implant interface and poor replacement of HA by bone may interfere with
Metal-on-metal (MOM) bearings for hip arthroplasty are increasing in popularity. Concern remains, however, regarding the potential toxicological effects of the metal ions which these bearings release. The serum levels of cobalt and chromium in 22 patients who had undergone MOM resurfacing arthroplasty were compared with a matched group of 22 patients who had undergone 28 mm MOM total hip arthroplasty (THA). At a median of 16 months (7 to 56) after resurfacing arthroplasty, we found the median serum levels of cobalt and chromium to be 38 nmol/l (14 to 44) and 53 nmol/l (23 to 165) respectively. These were significantly greater than the levels after 28 mm MOM THA which were 22 nmol/l (15 to 87, p = 0.021) and 19 nmol/l (2 to 58, p <
0.001) respectively. Since the upper limit for normal patients without implants is typically 5 nmol/l, both groups had significantly raised levels of metal ions. MOM bearings of large diameter, however, result in a greater systemic exposure of cobalt and chromium ions than bearings of small diameter. This may be of relevance for potential
Mononuclear osteoclast precursors are present in the wear-particle-associated macrophage infiltrate found in the membrane surrounding loose implants. These cells are capable of differentiating into osteoclastic bone-resorbing cells when co-cultured with the rat osteoblast-like cell line, UMR 106, in the presence of 1,25(OH). 2. vitamin D. 3. In order to develop an in vitro model of osteoclast differentiation which more closely parallels the cellular microenvironment at the bone-implant interface in situ, we determined whether osteoblast-like human bone-derived cells were capable of supporting the differentiation of osteoclasts from arthroplasty-derived cells and analysed the humoral conditions required for this to occur.
The clinical use of hydroxyapatite (HA) coating is controversial especially in regard to the
Gene therapy with insulin-like growth factor-1 (IGF-1) increases matrix production and enhances chondrocyte proliferation and survival in vitro. The purpose of this study was to determine whether arthroscopically-grafted chondrocytes genetically modified by an adenovirus vector encoding equine IGF-1 (AdIGF-1) would have a beneficial effect on cartilage healing in an equine femoropatellar joint model. A total of 16 horses underwent arthroscopic repair of a single 15 mm cartilage defect in each femoropatellar joint. One joint received 2 × 10. 7. AdIGF-1 modified chondrocytes and the contralateral joint received 2 × 10. 7. naive (unmodified) chondrocytes. Repairs were analysed at four weeks, nine weeks and eight months after surgery. Morphological and histological appearance, IGF-1 and collagen type II gene expression (polymerase chain reaction, in situ hybridisation and immunohistochemistry), collagen type II content (cyanogen bromide and sodium dodecyl sulphate-polyacrylamide gel electrophoresis), proteoglycan content (dimethylmethylene blue assay), and gene expression for collagen type I, matrix metalloproteinase (MMP)-1, MMP-3, MMP-13, aggrecanase-1, tissue inhibitor of matrix metalloproteinase-1 (TIMP-1) and TIMP-3 were evaluated. Genetic modification of chondrocytes significantly increased IGF-1 mRNA and ligand production in repair tissue for up to nine weeks following transplantation. The gross and histological appearance of IGF-1 modified repair tissue was improved over control defects. Gross filling of defects was significantly improved at four weeks, and a more hyaline-like tissue covered the lesions at eight months. Histological outcome at four and nine weeks post-transplantation revealed greater tissue filling of defects transplanted with genetically modified chondrocytes, whereas repair tissue in control defects was thin and irregular and more fibrous. Collagen type II expression in IGF-1 gene-transduced defects was increased 100-fold at four weeks and correlated with increased collagen type II immunoreaction up to eight months. Genetic modification of chondrocytes with AdIGF-1 prior to transplantation improved early (four to nine weeks), and to a lesser degree
Aternatives to autogenous bone graft for spinal fusion have been investigated for many years. It has been shown that osteoconductive materials alone do not give a rate of fusion which is comparable to that of autogenous bone graft. We analysed the effectiveness of porous ceramic loaded with cultured mesenchymal stem cells as a new graft material for spinal fusion in an animal model. Posterolateral fusion was carried out at the L4/L5 level in 40 White New Zealand rabbits using one of the following graft materials: porous ceramic granules plus cultured mesenchymal stem cells (group I); ceramic granules plus fresh autogenous bone marrow (group II); ceramic granules alone (group III); and autogenous bone graft (group IV). The animals were killed eight weeks after surgery and the spines were evaluated radiographically, by a manual palpation test and by histological analysis. The rate of fusion was significantly higher in group I compared with group III and higher, but not significantly, in group I compared with groups II and IV. In group I histological analysis showed newly formed bone in contact with the implanted granules and highly cellular bone marrow between the newly formed trabecular bone. In group II, thin trabeculae of newly formed bone were present in the peripheral portion of the fusion mass. In group III, there was a reduced mount of newly formed bone and abundant fibrous tissue. In group IV, there were thin trabeculae of newly formed bone close to the decorticated transverse processes and dead trabecular bone in the central portion of the fusion mass. In vitro cultured mesenchymal stem cells may be loaded into porous ceramic to make a graft material for spinal fusion which appears to be more effective than porous ceramic alone. Further studies are needed to investigate the medium- to
Extracorporeal shock-wave (ESW) treatment hasbeen shown to be effective in promoting the healing of fractures. We aimed to determine whether ESW could enhance the growth of bone-marrow osteoprogenitor cells. We applied ESW to the left femur of rats 10 mm above the knee at 0.16 mJ/mm. 2. in a range of between 250 and 2000 impulses. Bone-marrow cells were harvested after ESW for one day and subjected to assessment of colony-forming unit (CFU) granulocytes, monocytes, erythocytes, megakaryocytes (CFU-Mix), CFU-stromal cells (CFU-S) and CFU-osteoprogenitors (CFU-O). We found that the mean value for the CFU-O colonies after treatment with 500 impulses of ESW was 168.2 CFU-O/well (. sem. 11.3) compared with 88.2 CFU-O/well (. sem. 7.2) in the control group. By contrast, ESW treatment did not affect haematopoiesis as shown by the CFU-Mix (p = 0.557). Treatment with 250 and 500 impulses promoted CFU-O, but not CFU-Mix formations whereas treatment with more than 750 impulses had an inhibiting effect. Treatment with 500 impulses also enhanced the activity of bone alkaline phosphatase in the subculture of CFU-O (p<
0.01), indicating a selective promotion of growth of osteoprogenitor cells. Similarly, formation of bone nodules in the
The treatment of chronic osteomyelitis often
includes surgical debridement and filling the resultant void with antibiotic-loaded
polymethylmethacrylate cement, bone grafts or bone substitutes.
Recently, the use of bioactive glass to treat bone defects in infections
has been reported in a limited series of patients. However, no direct comparison
between this biomaterial and antibiotic-loaded bone substitute has
been performed. In this retrospective study, we compared the safety and efficacy
of surgical debridement and local application of the bioactive glass
S53P4 in a series of 27 patients affected by chronic osteomyelitis
of the long bones (Group A) with two other series, treated respectively
with an antibiotic-loaded hydroxyapatite and calcium sulphate compound
(Group B; n = 27) or a mixture of tricalcium phosphate and an antibiotic-loaded
demineralised bone matrix (Group C; n = 22). Systemic antibiotics
were also used in all groups. After comparable periods of follow-up, the control of infection
was similar in the three groups. In particular, 25 out of 27 (92.6%)
patients of Group A, 24 out of 27 (88.9%) in Group B and 19 out
of 22 (86.3%) in Group C showed no infection recurrence at means
of 21.8 (12 to 36), 22.1 (12 to 36) and 21.5 (12 to 36) months follow-up,
respectively, while Group A showed a reduced wound complication
rate. Our results show that patients treated with a bioactive glass
without local antibiotics achieved similar eradication of infection
and less drainage than those treated with two different antibiotic-loaded
calcium-based bone substitutes. Cite this article:
We analysed the effects of commonly used medications
on human osteoblastic cell activity in vitro, specifically proliferation
and tissue mineralisation. A list of medications was retrieved from
the records of patients aged >
65 years filed in the database of
the largest health maintenance organisation in our country (>
two
million members). Proliferation and mineralisation assays were performed
on the following drugs: rosuvastatin (statin), metformin (antidiabetic),
metoprolol (β-blocker), citalopram (selective serotonin reuptake
inhibitor [SSRI]), and omeprazole (proton pump inhibitor (PPI)).
All tested drugs significantly stimulated DNA synthesis to varying
degrees, with rosuvastatin 5 µg/ml being the most effective among
them (mean 225% ( Cite this article:
For the treatment of ununited fractures, we developed
a system of delivering magnetic labelled mesenchymal stromal cells
(MSCs) using an extracorporeal magnetic device. In this study, we
transplanted ferucarbotran-labelled and luciferase-positive bone
marrow-derived MSCs into a non-healing femoral fracture rat model
in the presence of a magnetic field. The biological fate of the
transplanted MSCs was observed using luciferase-based bioluminescence
imaging and we found that the number of MSC derived photons increased
from day one to day three and thereafter decreased over time. The
magnetic cell delivery system induced the accumulation of photons at
the fracture site, while also retaining higher photon intensity
from day three to week four. Furthermore, radiological and histological
findings suggested improved callus formation and endochondral ossification.
We therefore believe that this delivery system may be a promising
option for bone regeneration.