Recent studies on large diameter femoral head hip replacements have implicated the modular taper junction as one of the significant sources of wear and corrosion products and this has been attributed to increased torque and bending on the taper interface. The aim of this study was to assess the effect of frictional torque and bending moment on fretting corrosion at the taper junction and to investigate whether different material combinations also had an effect. We examined 1) Cobalt Chromium (CoCr) heads on CoCr stems 2) CoCr heads on Titanium alloy (Ti) stems and 3) Ceramic heads on CoCr stems. In test 1 increasing torque was imposed by offsetting the femoral stem in the anterior posterior plane in increments of 0 mm, 4 mm, 6 mm and 8 mm where the force generated was equivalent to 0Nm, 9Nm, 14Nm and 18Nm. In Test 2 we investigated the effect of increasing bending moment by offsetting the application of axial load from the midline in the medial-lateral (ML). Offset increments equivalent to +0, +7 and +14 heads were used. For each test we used n=3 for each different material combination.Introduction
Patients/Materials & Methods
Cross linked polyethylene (XLPE) has gained popularity as a bearing surface of choice for younger patients despite only medium term results being available for wear rates. Concern remains regarding the long-term stability and durability of these materials. In order to address these issues we present the longest radiological and clinical follow-up of XLPE. Since 1986, we have prospectively studied a group of 17 patients (19 hips) that underwent a cemented Charnley low friction arthroplasty using a combination of 22.225mm alumina ceramic femoral head, a modified Charnley flanged stem and a chemically cross-linked polyethylene cup. We now report the 28 year clinical and radiological results.Introduction
Patients/Materials & Methods
This study investigates head-neck taper corrosion with varying head size in a novel hip simulator instrumented to measure corrosion related electrical activity under torsional loads. In all, six 28 mm and six 36 mm titanium stem-cobalt chrome head pairs with polyethylene sockets were tested in a novel instrumented hip simulator. Samples were tested using simulated gait data with incremental increasing loads to determine corrosion onset load and electrochemical activity. Half of each head size group were then cycled with simulated gait and the other half with gait compression only. Damage was measured by area and maximum linear wear depth.Aims
Methods
An ongoing prospective study to investigate failing metal-on-metal
hip prostheses was commenced at our centre in 2008. We report on
the results of the analysis of the first consecutive 126 failed
mated total hip prostheses from a single manufacturer. Analysis was carried out using highly accurate coordinate measuring
to calculate volumetric and linear rates of the articular bearing
surfaces and also the surfaces of the taper junctions. The relationship
between taper wear rates and a number of variables, including bearing
diameter and orientation of the acetabular component, was investigated.Objectives
Methods