Yoneo T Nakao M Sakai R Fukushima K Uchiyama K Takahira N Mabuchi K
Full Access

Introduction

On the basis of a proposal by Noble, the marrow cavity form can be classified into three categories: normal, champagne-fluted and stovepipe. In the present study, three typical finite element femoral models were created using CT data based on Noble's three categories. The purpose was to identify the relationship of stress distribution of the surrounding areas between femoral bone marrow cavity form and hip stems. The results shed light on whether the distribution of the high-stress area reflects the stem design concept. In order to improve the results of THA, researchers need to consider the instability of a stem design based on the stress distributioin and give feedback on future stem selection.

Methods

As analyzing object, we selected SL-PLUS and BiCONTACT stems. To develop finite element models, two parts (cortical bone and stem) were constructed using four-node tetrahedral elements. The model consisted of about 60,000 elements. The material characteristics were defined by the combination of mass density, elastic coefficient, and Poisson's ratio. Concerning the analysis system, HP Z800 Workstation was used as hardware and LS-DYNA Ver. 971 as software. The distal end of the femur was constrained in all directions. On the basis of ISO 7206 Part 4,8 that specifies a method of endurance testing for joint prostheses, the stem was tilted 10°, and a 1500 N resultant force in the area around the hip joint was applied to the head at an angle of 25° with the long axis. Automatic contact with a consideration of slip was used.


Orthopaedic Proceedings
Vol. 98-B, Issue SUPP_9 | Pages 76 - 76
1 May 2016
Nakao M Uchida K Sakai R Naruse K Takaso M Mabuchi K
Full Access

Background

Residual stress remains in bone tissues after press-fit-fixation of a joint prosthesis, recently employed for joint arthroplasty. The response of bone tissues to the residual stress is, however, unknown because it is not physiological. This unnatural stimulus may have adverse effects on bone tissues, including causing thigh pain or bone resorption. In the present study, we designed an experimental method to apply a stationary load from inside an animal femur using a loop spring of titanium alloy with super elasticity. The femoral response was assessed based on the migration of the wire into bone twelve weeks after implantation. As the results, wire migration was noted in 10 of 11 cases.

Methods

We developed a method using a loop spring made of super elastic titanium alloy, which can maintain sufficient stress in a rat femur for a prolonged period. This titanium alloy, which contains 43.94% titanium and 56.06% nickel, was supplied as a wire (WDL1, Actment Co., Ltd., Kasukabe, Japan). In the present study, an experimental method was designed to apply a stationary load from inside a rat femur by inserting a loop spring made of super elastic wire.


Orthopaedic Proceedings
Vol. 98-B, Issue SUPP_3 | Pages 79 - 79
1 Jan 2016
Nakao M Fukushima K Sakai R Takahira N Uchiyama K Yamamoto T Moriya M Mabuchi K
Full Access

Introduction

On the basis of a proposal by Noble, the marrow cavity form can be classified into three categories: stovepipe, normal, and champagne-fluted. In the present study, three typical finite element femoral models were created using CT data based on Noble's three categories. The purpose was to identify the relationship of stress distribution of the surrounding areas between femoral bone marrow cavity form and hip stem. The results shed light on whether the distribution of the high-stress area reflects the stem design concept. In order to improve the results of THA, researchers need to consider the instability of a stem design based on the pressure zone and give feedback on future stem selection.

Methods

To develop finite element models, two parts (cortical bone and stem) were constructed using four-node tetrahedral elements. The model consisted of about 40,000 elements. The material characteristics were defined by the combination of mass density, elastic coefficient, and Poisson's ratio. Concerning the analysis system, HP Z800 Workstation(HP, Japan) was used as hardware and LS-DYNA Ver. 971 (Livermore Software Technology Corporation, USA) as software. The distal end of the femur was constrained in all directions. On the basis of ISO 7206 Part 4,8 that specifies a method of endurance testing for joint prostheses, the stem was tilted 10°, and a 500 N resultant force in the area around the hip joint was applied to the head at an angle of 25° with the long axis. Automatic contact with a consideration of slip was used. Von Mises stress during a 1.0 s period after loading was analyzed, and stress distribution in the stem and its maximum value were calculated.


Orthopaedic Proceedings
Vol. 98-B, Issue SUPP_3 | Pages 2 - 2
1 Jan 2016
Mabuchi K Uchida K Ito T Shimizu K Nakao M Naruse K Sakai R
Full Access

INTRODUCTION

It is generally accepted that strong hammering is necessary for the press fit fixation of a joint prosthesis. In this regard, large stress must remain within bone tissues for a long period. This residual stress is, however, some different from the feasible mechanical stimuli for bone tissues because that is stationary, continuous and directed from within outward unlike physiological conditions. The response on this residual stress, which may induce the disorder of the fixation of implant, has not been discussed, yet.

In the present study, we designed an experimental method to exert a stationary load from inside of a femur of a rat by inserting a loop spring made from a super elastic wire of titanium alloy. Response of the femur was assessed by bone morphology mainly about the migration of the wire into the bone twelve weeks after the implantation.

MATERIALS AND METHODS

We developed a method using a loop spring made of super elastic wire of titanium alloy, which can maintain sufficient magnitude of stress in a rat femur during the experimental period. The loop spring was fabricated with a wire of 0.4 mm diameter before the quenching process. Eleven Wistar rats of ten weeks old were used for the experiments. The loop spring was inserted the right femur, as shown in Figure 1. The left femur was remained intact. The compressive load was added from within outward of bone marrow when the spring was compressed with the insertion into a bone marrow of a rat femur, as shown in Figure 2. The average contact stress was calculated by dividing the elastic force by the spring and bone contact area. The contact stress was distributed from 62 to 94 MPa, which are sufficiently lower than the yield stress of cortical bone [1]. The assessment of bone morphology around the implanted loop spring was performed by micro-CT imaging after the twelve weeks of cage activity.