Abstract
We compared the mechanical properties of normal and reconstructed heel pads in seven patients. Four had latissimus dorsi flaps and one each an anterior thigh flap, a local dorsalis pedis flap and a sural arterial flap.
The thickness of the heel pad was measured under serial incremental loads of 0.5 kg to a maximum of 3 kg and then relaxed sequentially. The load-displacement curve of the heel pad during a loading-unloading cycle was plotted and from this the unloaded heel-pad thickness (UHPT), compressibility index (CI), elastic modulus (Ep), and energy dissipation ratio (EDR) were calculated.