The peri-prosthetic tissue response to wear debris
is complex and influenced by various factors including the size, area
and number of
Aims. Vitamin E-infused highly cross-linked polyethylene (E1) has recently been introduced in total knee arthroplasty (TKA). An in vitro wear simulator study showed that E1 reduced polyethylene wear. However there is no published information regarding in vivo wear. Previous reports suggest that newly introduced materials which reduce in vitro polyethylene wear do not necessarily reduce in vivo polyethylene wear. To assist in the evaluation of the newly introduced material before widespread use, we established an in vivo polyethylene wear
We revised seven alumina-blasted cementless hip prostheses (Ti-alloy stems, cp Ti threaded sockets) with low- or high-carbon Co-alloy bearings at a mean of 20.1 months after implantation because of pain and loosening. Histological examination of the retrieved periprosthetic tissues from two cases in which the implant was stable and three in which the socket was loose showed macrophages with basophilic granules containing metal and alumina wear
Objectives. This study aimed to characterise and qualitatively grade the severity of the corrosion
In an attempt to increase the life of cementless prostheses, an hydroxyapatite-coated implant which releases a bisphosphonate has been suggested as a drug-delivery system. Our in vitro study was designed to determine the maximum dose to which osteoblasts could be safely exposed. Our findings demonstrated that zoledronate did not impair the proliferation of human osteoblasts when used at concentrations below 1 μ. m. Murine cells can be exposed to concentrations as high as 10 μ. m. . A concentration of 0.01% of titanium
Nanometre-sized
Despite many claims of good wear properties following
total knee replacement (TKR) with an oxidised zirconium (OxZr) femoral
component, there are conflicting clinical results. We hypothesised
that there would be no difference in either the mid-term clinical
and radiological outcomes or the characteristics of the polyethylene
wear
Abundant implant-derived biomaterial wear
The biological significance of cobalt-chromium wear
We investigated in vitro a mechanism by which particulate debris may induce bone resorption and cause implant loosening. We first studied two standard
Tissue reaction to wear
We implanted bone harvest chambers (BHCs) bilaterally in ten mature male New Zealand white rabbits. Polyethylene
Although the response of macrophages to polyethylene debris has been widely studied, it has never been compared with the cellular response to ceramic debris. Our aim was to investigate the cytotoxicity of ceramic
We used a rat model in vivo to study the effects of the concentration of polyethylene
We analysed revised Mathys isoelastic polyacetal femoral stems with stainless-steel heads and polyethylene acetabular cups from eight patients in order to differentiate various types of
We have studied the beneficial effects of a hydroxyapatite (HA) coating on the prevention of the migration of wear debris along the implant-bone interface. We implanted a loaded HA-coated implant and a non-coated grit-blasted titanium alloy (Ti) implant in each distal femoral condyle of eight Labrador dogs. The test implant was surrounded by a gap communicating with the joint space and allowing access of joint fluid to the implant-bone interface. We injected polyethylene (PE)
Particulate wear debris is associated with periprosthetic inflammation and loosening in total joint arthroplasty. We tested the effects of titanium alloy (Ti-alloy) and PMMA
Wear
Reports of differing failure rates of total hip prostheses made of various metals prompted us to measure the size of metallic and polyethylene particulate debris around failed cemented arthroplasties. We used an isolation method, in which metallic debris was extracted from the tissues, and a non-isolation method of routine preparation for light and electron microscopy. Specimens were taken from 30 cases in which the femoral component was of titanium alloy (10), cobalt-chrome alloy (10), or stainless steel (10). The mean size of metallic
Sterilisation by gamma irradiation in the presence of air causes free radicals generated in polyethylene (PE) to react with oxygen, which could lead to loss of physical properties and reduction in fatigue strength. Tissue retrieved from failed total hip replacements often has large quantities of particulate PE and most