Objectives. An experimental piglet model induces avascular necrosis (AVN)
and deformation of the
Objectives. Circulating exosomes represent novel biomarkers for multiple diseases. In this study, we investigated whether circulating exosome levels could be used as a diagnostic biomarker for steroid-induced osteonecrosis of the
The efficacy of β-tricalcium phosphate (β-TCP) loaded with bone morphogenetic protein-2 (BMP-2)-gene-modified bone-marrow mesenchymal stem cells (BMSCs) was evaluated for the repair of experimentally-induced osteonecrosis of the
In spite of extensive accounts describing the blood supply to the
In about 50% of cases, osteonecrosis of the
We used laser Doppler flowmetry (LDF) with a high energy (20 mW) laser to measure perfusion of the
The use of a composite osteochondral device for simulating partial hemiarthroplasty was examined. The device was composed of a polyvinyl alcohol hydrogel and a titanium fibre mesh, acting as artificial cartilage and as porous artificial bone, respectively. The titanium fibre mesh was designed to act as an interface material, allowing firm attachment to both the polyvinyl alcohol gel (through injection moulding) and the femoral joint surface (through bony ingrowth). We implanted 22 of these devices into canine
Osteonecrosis of the
From November 1994 to March 1997, we harvested 137 grafts of the
We examined stainless-steel, cobalt-chrome, titanium and alumina and zirconia ceramic
In this prospective, randomised study, we have compared the wear rate of cemented, acetabular polyethylene cups articulating with either a 22 mm or a 32 mm cobalt-chromium head. We evaluated 89 patients who had a total of 484 radiographs. The mean follow-up period was 71.4 months (SD 29.1). All the radiographs were digitised and electronically measured. The linear wear rate was significantly higher during the first two years and decreased after this period to a constant value. We suggest that this is partly due to a ‘run-in’ process caused by irregularities between surfaces of the cup and head and an initial plastic deformation of the polyethylene. The mean volumetric wear was 120.3 mm3/year for the 32 mm head, which was significantly higher than the 41.5 mm3/year for the 22 mm heads. The mean linear wear rate was not significantly different. We were, however, unable to find radiological signs of osteolysis in the patients who had higher wear rates.
Objectives. Intramedullary fixation is considered the most stable treatment for pertrochanteric fractures of the proximal femur and cut-out is one of the most frequent mechanical complications. In order to determine the role of clinical variables and radiological parameters in predicting the risk of this complication, we analysed the data pertaining to a group of patients recruited over the course of six years. Methods. A total of 571 patients were included in this study, which analysed the incidence of cut-out in relation to several clinical variables: age; gender; the AO Foundation and Orthopaedic Trauma Association classification system (AO/OTA); type of nail; cervical-diaphyseal angle; surgical wait times; anti-osteoporotic medication; complete post-operative weight bearing; and radiological parameters (namely the lag-screw position with respect to the
We investigated the antibiotic concentration in fresh-frozen
In order to investigate the osteoinductive properties of allograft used in impaction grafting and the effect of strain during impaction on these properties, we designed an in vitro experiment to measure strain-related release of bone morphogenetic protein-7 (BMP-7) from fresh-frozen
Objectives. We studied subchondral intraosseous pressure (IOP) in an animal model during loading, and with vascular occlusion. We explored bone compartmentalization by saline injection. Materials and Methods. Needles were placed in the femoral condyle and proximal tibia of five anaesthetized rabbits and connected to pressure recorders. The limb was loaded with and without proximal vascular occlusion. An additional subject had simultaneous triple recordings at the
Objectives. Taper junctions between modular hip arthroplasty
We have reviewed 70 patients with bilateral simultaneous total hip arthroplasties to determine the rate of failure and to compare polyethylene wear and osteolysis between an implant with a cobalt-chrome head and Hylamer liner with that of a zirconia head and Hylamer liner. The mean thickness of the polyethylene liner was 11.0 mm (8.8 to 12.2) in the hip with a zirconia head and 10.7 mm (8.8 to 12.2) in that with a cobalt-chrome head. At follow-up at 6.4 years no acetabular or femoral component had been revised for aseptic loosening and no acetabular or femoral component was loose according to radiological criteria in both the cemented and cementless groups. The mean rate of linear wear and annual wear rate were highest in the 22 mm zirconia
Treatment with corticosteroids is a risk factor for non-traumatic avascular necrosis of the