Periasamy K Watson WS Mohammed A Murray H Walker B Patil S Meek RMD

The ideal acetabular component is characterised by reliable, long-term fixation with physiological loading of bone and a low rate of wear. Trabecular metal is a porous construct of tantalum which promotes bony ingrowth, has a modulus of elasticity similar to that of cancellous bone, and should be an excellent material for fixation.

Between 2004 and 2006, 55 patients were randomised to receive either a cemented polyethylene or a monobloc trabecular metal acetabular component with a polyethylene articular surface. We measured the peri-prosthetic bone density around the acetabular components for up to two years using dual-energy x-ray absorptiometry.

We found evidence that the cemented acetabular component loaded the acetabular bone centromedially whereas the trabecular metal monobloc loaded the lateral rim and behaved like a hemispherical rigid metal component with regard to loading of the acetabular bone. We suspect that this was due to the peripheral titanium rim used for the mechanism of insertion.


The Journal of Bone & Joint Surgery British Volume
Vol. 89-B, Issue 9 | Pages 1158 - 1164
1 Sep 2007
Lusty PJ Watson A Tuke MA Walter WL Walter WK Zicat B

We studied 33 third generation, alumina ceramic-on-ceramic bearings retrieved from cementless total hip replacements after more than six months in situ. Wear volume was measured with a Roundtest machine, and acetabular orientation from the anteroposterior pelvic radiograph. The overall median early wear rate was 0.1 mm3/yr for the femoral heads, and 0.04 mm3/yr for the acetabular liners. We then excluded hips where the components had migrated. In this stable subgroup of 22 bearings, those with an acetabular anteversion of < 15° (seven femoral heads) had a median femoral head wear rate of 1.2 mm3/yr, compared with 0 mm3/yr for those with an anteversion of ≥15° (15 femoral heads, p < 0.001). Even under edge loading, wear volumes with ceramic-on-ceramic bearings are small in comparison to other bearing materials. Low acetabular anteversion is associated with greater wear.