Concerns regarding UHMWPE wear particle induced osteolysis in total hip replacement (THR, [1]) have led to alternative materials to be sought. Carbon-fibre reinforced poly-ether-ether-ketone (CFR-PEEK) has shown reduced wear in hip and knee configurations compared with conventional polyethylene [2-4]. The aim of this study was to investigate the wear performance of a ceramic-on-CFR PEEK THR through a simulator study. Five 36mm diameter Biolox Delta heads were paired with extruded CFR-PEEK cups and tested in a hip wear simulator (Simulator Solutions, UK) for 10 million cycles (Mc). Tests were performed in a Prosim hip simulator, which applied a twin peak loading cycle, with a peak load of 3kN. Flexion-extension of −15 to +30 degrees was applied to the head and internal-external rotation of +/− 10 degrees was applied to the cup, components were mounted anatomically. The lubricant was 25% (v/v) calf serum supplemented with 0.03% (w/v) sodium azide. Wear was assessed gravimetrically at several intervals adjusted for moisture uptake using loaded and unloaded soak controls.Introduction
Methodology