Abstract
We studied the calcium content and mechanical strength of cortical bone from rats and dogs after different periods of demineralisation, showing that the rate of demineralisation differed considerably between the species. Specimens from the rat were further treated by chemical extraction and autolysis and tested for osteoinductive properties. We showed that partially demineralised cortical bone retained adequate mechanical strength, while retaining the biological effects of completely demineralised bone. This shows that it is possible to prepare allografts which have adequate mechanical strength and still retain osteo-inductive properties.