A modular layered acetabular component (metal-polyethylene-ceramic) was developed in Japan for use in
Aims. Our aim in this study was to describe a continuing review of
11 total hip arthroplasties using 22.225 mm
It has been suggested that the wear of ultra-high molecular weight polyethylene (UHMWPE) in total hip replacement is substantially reduced when the femoral head is ceramic rather than metal. However, studies of
Aims. To determine the effect of a change in design of a cementless
ceramic acetabular component in fixation and clinical outcome after
total hip arthroplasty. Patients and Methods. We compared 342 hips (302 patients) operated between 1999 and
2005 with a relatively smooth hydroxyapatite coated acetabular component
(group 1), and 337 hips (310 patients) operated between 2006 and
2011 using a similar acetabular component with a macrotexture on
the entire outer surface of the component (group 2). The mean age of
the patients was 53.5 (14 to 70) in group 1 and 53.0 (15 to 70)
in group 2. The mean follow-up was 12.7 years (10 to 17) for group
1 and 7.2 years (4 to 10) for group 2. Results. No hips were revised due to complications related to bearing
fracture or to stem loosening. A total of 15 acetabular components
were revised for aseptic loosening in group 1 and two in group 2.
The survival rate for acetabular component aseptic loosening at
eight years was 96.8% (95% confidence interval (CI) 94.8 to 98.7)
for group 1 and 99.2% (95% CI 98.0 to 100) for group 2. The risk
for aseptic loosening of the acetabular component was higher in group
1 (p = 0.04, Hazard Ratio (HR) 4.99), dysplastic acetabula (p =
0.01, HR 4.12), components outside Lewinnek´s zone (p <
0.001,
HR 6.13) and in those with a hip rotation centre distance greater
than 5 mm (p = 0.005, HR 4.09). . Conclusion.
We report the clinical and radiological outcomes
of a series of contemporary cementless ceramic-on-ceramic total hip
replacements (THRs) at ten years in patients aged ≤ 55 years of
age. Pre- and post-operative activity levels are described. A total
of 120 consecutive ceramic cementless THRs were performed at a single
centre in 110 patients from 1997 to 1999. The mean age of the patients
at operation was 45 years (20 to 55). At ten years, four patients
had died and six were lost to follow-up, comprising ten hips. The
mean post-operative Harris hip score was 94.7 (55 to 100). Radiological
analysis was undertaken in 90 available THRs of the surviving 106
hips at final review: all had evidence of stable bony ingrowth,
with no cases of osteolysis. Wear was undetectable. There were four
revisions. The survival for both components with revision for any
cause as an endpoint was 96.5% (95% confidence interval 94.5 to
98.7). The mean modified University of California, Los Angeles activity
level rose from a mean of 6.4 (4 to 10) pre-operatively to 9.0 (6
to 10) at the ten-year post-operative period.
Although
This multicentre study analysed 12
We examined the behaviour of
We report the results of our continued review of 11 total hip arthroplasties using 22.225 mm
Between 1990 and 1992, we implanted 71 hybrid alumina-on-alumina hip arthroplasties in 62 consecutive patients under the age of 55 years, with a mean age of 46 years at surgery. There were 56 primary and 15 secondary procedures. The prostheses involved a cemented titanium alloy stem, a 32 mm
We report the results of our continued review of 14 hip arthroplasties using
The aim of this study was to report the mid-term clinical outcome
of cemented unlinked J-alumina ceramic elbow (JACE) arthroplasties
when used in patients with rheumatoid arthritis (RA). We retrospectively reviewed 87 elbows, in 75 patients with RA,
which was replaced using a cemented JACE total elbow arthroplasty
(TEA) between August 2003 and December 2012, with a follow-up of
96%. There were 72 women and three men, with a mean age of 62 years
(35 to 79). The mean follow-up was nine years (2 to 14). The clinical condition
of each elbow before and after surgery was assessed using the Mayo
Elbow Performance Index (MEPI, 0 to 100 points). Radiographic loosening
was defined as a progressive radiolucent line of >1 mm that was
completely circumferential around the prosthesis.Aims
Patients and Methods
We report the clinical and tribological performance of 67 ceramic acetabular prostheses implanted between 1976 and 1979 without bone cement. They articulated with ceramic femoral heads mounted on mental femoral stems. After a mean elapsed period of 144 months, 59 sockets were radiographically stable but two showed early signs and six showed late signs of loosening. Four of the loose sockets have been revised. Histological analysis of the retrieved tissue showed a fibrous membrane around all the implants, with fibrocartilage in some. There was no bone ingrowth, and the fibrous membrane was up to 6 mm thick and infiltrated with lymphocytes, plasma cells, and macrophages. Intra- and extracellular birefringent wear particles were seen. Tribological analysis showed total wear rates in two retrieved alumina-on-alumina joints of 2.6 microns per year in a stable implant and 68 microns in a loose implant. Survival analysis showed a revision rate of 12.4% at 136 months.
From 1981 to 1983, we implanted Bioceram type-4 and type-5 prostheses in 61 hips in 54 patients with osteoarthritis secondary to acetabular dysplasia, congenital subluxation, or congenital dislocation of the hip. Fifty-seven hips in 50 patients were followed for a mean of 11.1 years (10 to 13). The mean age of the patients at operation was 53 years (31 to 70). Functional evaluation using the Merle d'Aubigne and Postel hip score showed a 77% success rate. Radiological loosening occurred in three femoral (5%) and 16 acetabular components (28%). Autologous femoral head grafts were used in 18 hips and became incorporated, giving mechanical support to the socket except for one which occupied a large weight-bearing area and eventually collapsed. The mean polyethylene wear was 1.1 mm (0 to 3.6) and the mean wear rate was 0.10 mm/year (0 to 0.31). A high rate of wear correlated with calcar resorption (p >
0.002) but not with acetabular loosening. There was no breakage of a ceramic head. Study of the ceramic heads and polyethylene sockets retrieved after ten years showed excellent surface roughness, sphericity, and bending strength for the heads but scratches and voids were seen on the sockets.
We report the findings from independent prospective clinical and laboratory-based joint-simulator studies of the performance of ceramic femoral heads of 22.225 mm diameter in cross-linked polyethylene (XLP) acetabular cups. We found remarkable qualitative and quantitative agreement between the clinical and simulator results for the wear characteristics with time, and confirmed that ceramic femoral heads penetrate the XLP cups at only about half the rate of otherwise comparable metal heads. In the clinical study, 19 hips in 17 patients were followed for an average of 77 months. In the hip-joint simulator a similar prosthesis was tested for 7.3 million cycles. Both clinical and simulator results showed relatively high rates of penetration over the first 18 months or 1.5 million cycles, followed by a very much lower wear thereafter. Once an initial bedding-in of 0.2 mm to 0.4 mm had taken place the subsequent rates of penetration were very small. The initial clinical wear during bedding-in averaged 0.29 mm/year; subsequent progression was an order of magnitude lower at about 0.022 mm/year, lower than the 0.07 mm/year in metal-to-UHMWP Charnley LFAs. Our results show the excellent tribological features of alumina-ceramic-to-XLP implants, and also confirm the value of well-designed joint simulators for the evaluation of total joint replacements.
We describe a model which can be used for in vitro biocompatibility assays of biomaterials. We studied the in vitro response of human osteoarthritis or rheumatoid arthritis fibroblast-like synoviocytes to Al2O3 or ZrO2 particles by analyzing the production of interleukin-1 (IL-1) and interleukin-6 (IL-6) and the metabolism of arachidonic acid via lipoxygenase and cyclo-oxygenase pathways. Our results show that, in these cells and under our experimental conditions, Al2O3 and ZrO2 did not significantly modify the synthesis of IL-1 and IL-6 or the metabolism of arachidonic acid.
Our aim in this prospective study was to compare the bone mineral density (BMD) around cementless acetabular and femoral components which were identical in geometry and had the same
Aims. The aim of this study was to conduct the largest low contact stress (LCS) retrieval study to elucidate the failure mechanisms of the Porocoat and Duofix femoral component. The latter design was voluntarily recalled by the manufacturer. Materials and Methods. Uncemented LCS explants were divided into three groups: Duofix, Porocoat, and mixed. Demographics, polyethylene wear, tissue ingrowth, and metallurgical analyses were performed. Results. In 104 implants, a decrease in the odds of loosening and an increase in metallosis and tissue staining in the Duofix group relative to Porocoat group was detected (p = 0.028). There was an increased presence of embedded metallic debris in the Duofix group (p < 0.001). Decreased tissue ingrowth was associated with the Duofix surface (p < 0.001). The attached beads had reduced microhardness, indicative of adverse thermal processing, which resulted in bead shedding, particulate debris, and metallosis. Conclusion. Hydroxyapatite coating of the LCS femoral component produced unexpected results and led to its recall. The root cause was likely a combination of retained
We present a retrospective series of 170 cemented titanium straight-stem femoral components combined with two types of femoral head: cobalt-chromium (CoCr) alloy (114 heads) and