Orthopaedic Proceedings
Vol. 98-B, Issue SUPP_7 | Pages 108 - 108
1 May 2016
De Villiers D Banfield S Housden J Shelton J
Full Access

Introduction

Revision of total hip replacements (THRS) is predominantly due to aseptic loosening, pain and infection [1]. The current method used to address the risk of infection is to administer antibiotics and to include antibacterial agents into bone cement (if used) and on implant coatings [2–4]. Currently, silver (Ag) coatings have only been applied to titanium hip stems [3]. Cobalt chromium alloy (CoCr) is a widely used orthopaedic alloy which is commonly used as a bearing surface; revisions of joints using this material often describe adverse reactions to the particulate wear debris [1]. This study considers an Ag containing CrN based coating on a CoCr substrate with the aim to reduce cobalt (Co) release and promote antibacterial silver release.

Methods

Silver Chromium Nitride (CrNAg) coatings were developed and applied onto the bearing surfaces of 48 mm diameter metal-on-metal THRs. Three coatings were evaluated: high Ag at the surface (CrNAg+), low Ag at surface (CrNAg-) and uniform Ag (CrNAg=). All bearings were tested under ISO 14242-3 conditions for 0.17 million cycles (mc) representing approximately 2 months use in vivo. Wear was determined gravimetrically; Ag and Co levels in the lubricant were measured using graphite furnace atomic absorption spectroscopy. Testing of the CrNAg= bearings were continued to 2mc under standard conditions; CrNAg- bearings to 5mc incorporating lateralisation, which created separation at swing phase and rim contact at heel strike. Wear volume and Ag/Co release were monitored at 0.33, 0.67, 1mc and every mc thereafter.


Orthopaedic Proceedings
Vol. 95-B, Issue SUPP_34 | Pages 281 - 281
1 Dec 2013
De Villiers D Kinbrum A Traynor A Collins S Banfield S Housden J Shelton J
Full Access

Introduction

Vitamin-E has been introduced into highly-crosslinked polyethylene liners to reduce the oxidation potential of the material while maintaining low wear rates. However, little has been reported on adverse testing of the material with one test on diffused vitamin-E polyethylene [1] and no adverse tests of vitamin-E blended polyethylene reported. Adverse testing of crosslinked polyethylene has focused on the use of large diameters, the incorporation of third body particles, roughening of the counterface or severe activity [2–4]. This investigation considers the wear of vitamin-E blended highly-crosslinked polyethylene under standard and adverse conditions articulating against uncoated and chromium nitride (CrN) coated metal heads.

Methods

Seven metal heads were tested against prototype ϕ52 mm 0.1 wt% vitamin-E blended highly-crosslinked polyethylene liners (Corin, UK). Three heads remained as cast double heat treated metal (MoP) while four, of similar metallurgy, were coated with CrN via electron beam physical vapour deposition (CrNoP) (Tecvac, UK) and polished to a similar surface finish. Tests were conducted for 5 million cycles (mc) under conditions described in ISO 14242–3: 2009. Alumina particles (mean size 2.4 μm) at concentrations of 0.15 mg/mL were added to the lubricant for 1 mc to consider the effect of severe head damage. Testing continued for a further 1 mc without the presence of the particles and then 3 jogging intervals (14,400 cycles each) were conducted at slow, medium and fast speeds [3]. Wear volume was determined gravimetrically for the heads and liners and fluid collected throughout the testing was analysed for cobalt concentration using graphite furnace atomic absorption spectroscopy.